Abstract:
热稳定性是非晶态合金应用中重要的性能之一。本文利用示差扫描量热法测定了Ni—7.6wt%Fe—13.7wt%P非晶态合金的DSC曲线。该合金在连续加热过程中发生了六次放热转变,峰值分别为248,303,322,350,376,442℃。322℃峰在快速加热中消失,其它五次放热转变的激活能分别为131.5,111.6,237.8,253.6,238.5kJ/mol。研究结果表明,Fe—Ni—P非晶态合金的热稳定性优于非晶态Ni—P合金。