3Y-TZP/Al2O3 composites were pressureless sintered with the addition of TiO2-MnO2 and CaO-Al 2O3-SiO2 glass. The densification, microstructure and mechanical properties of the composites were investigated. It was found that the composites could be densified at a temperature as low as 1400°C by liquid phase sintering. The majority of the grain sizes for both Al2O3 and ZrO2 were below 1 μm because of the lower sintering temperature. A bending strength of 934±28 MPa and fracture toughness of 7.82±0.19 MPam1/2 were obtained for 3Y-TZP/Al2O3 (20 vol%) composite. Transformation toughening is considered the responsible toughening mechanism. © 2005 Springer Science + Business Media, Inc.
Keyword:
Reprint 's Address:
Email:
Source :
Journal of Materials Science
ISSN: 0022-2461
Year: 2005
Issue: 7
Volume: 40
Page: 1693-1697
0 . 9 0 1
JCR@2005
3 . 5 0 0
JCR@2023
JCR Journal Grade:2
Cited Count:
SCOPUS Cited Count: 4
ESI Highly Cited Papers on the List: 0 Unfold All
WanFang Cited Count:
Chinese Cited Count:
30 Days PV: 0
Affiliated Colleges: