Abstract:
以室温电导率达10<''-4>S/cm的锂快离子导体Li<,1.5>Al<,0.1>Yb<,0.3>Ti<,1.6>Si<,0.1>P<,2.9>O<,12>(简称L031)为电解质、Mg为负极、V<,2>O<,5>和CuCl为复合正极、石墨为集流极来组装电池,电池的结构式为(g)Mg/L031/V<,2>O<,5>+CuCl(1:2)/C(石墨)(+)该电池在530kΩ的负载下放电时有一长的放电平台为1.80V.当放电电压截止到0.69V时电池的放电容量为4.12mAh,电池的重量比能量为12.79Wh/kg,当电池负载下降至100kΩ时,放电平台和重量比能量都大为下降.