Abstract:
以桃壳活性炭为载体,四乙烯五胺(TEPA)为改性剂,进行直接改性、HNO3氧化后改性,考察改性后活性炭的孔隙特征及其对CO2的吸附性能。实验表明:改性后,活性炭的比表面积和孔容减小,孔径增大。直接改性后,活性炭对CO2的吸附性能没有明显增加,HNO3+TEPA复合改性后,对CO2的吸附性能显著提高,303 K时,对CO2的吸附量从改性前的0.39 mmol/g提高到0.73 mmol/g。TE-PA的投药量影响复合改性效果,最佳投药量为20%。