采用固相合成法制备了(1-x)Ba4Sm9.33Ti18O54-xCa0.61Nd0.26TiO3[(1-x)BST-xCNT]系微波介质陶瓷.探讨了组成、烧结温度对微波介质陶瓷结构、介电性能的影响.x<0.6时,(1-x)BST-xCNT陶瓷为正交结构的新型钨青铜单相.x≥0.6时,相继出现了第二相Sm2Ti2O7和钙钛矿相,最终形成钙钛矿单相.微波介质陶瓷的介电常数ε随x的增大持续升高,品质因子Qf值则先增大后迅速减小再急剧增大.1 325~1 350 ℃烧结样品的微波介电性能达到最佳:x=0时,ε=75,Qf=8985GHz,谐振频率温度系数τf=-8.2×10-6/℃;x=0.2时,ε=75,Qf=9 552GHz,τf=-14.4×10-6/℃;x=1时,ε=108.9,Qf=14919GHz,τf=236.2×10-6/℃.