Na1+3x+yAlxNdyTi2-x-ySi2xP3-2xO12钠快离子导体(以下简称Al-Nd-Nasicon)可以用精选的天然叶腊石A12[Si4O10](OH)2为起始原料与其它化合物,经过高温(900~1100℃)固相反应约15h制得.在y=0.3,x≤0.3和y=0.5,x≤0.2的组成范围内可得到具有Nasicon的三方结构空间群属于R3C的固溶体.该相具有较高的电导率,其中起始组成y=0.3,x=0.1的合成物在350℃时电导率为1.80×10-2S/cm.