Abstract:
以钛酸正丁酯为原料,用溶胶-凝胶过程超临界CO2萃取法制备具有锐钛矿晶型结构的纳米TiO2气凝胶,用XRD、TEM、BET等分别对初生态气凝胶粒子、在常态下以气凝胶形式保存了360 d的TiO2纳米粒子及以初生态气凝胶的粉体保存了360 d的TiO2粒子进行表征,以光催化降解罗丹明B为模型反应.结果表明,以气凝胶形式保存纳米粒子能有力地防止纳米粒子的团聚,并基本保持初生态气凝胶粒子光催化降解罗丹明B的能力.