采用铁尾矿粉取代石英粉配制超高性能混凝土(ultra-high performance concrete, UHPC),研究不同养护制度下掺铁尾矿粉UHPC力学性能.结果表明:随铁尾矿粉取代率增加, UHPC流动度略有下降,力学性能基本不变;与标准养护相比,恒温水养和蒸压养护下掺铁尾矿粉UHPC抗压、抗折强度及折压比显著提升.结合微观试验结果发现,铁尾矿粉取代石英粉对水泥石显微硬度及孔结构无不利影响.恒温水养和蒸压养护下掺铁尾矿粉UHPC的水泥水化更充分,水化产物Ca/Si比值下降,水泥石显微硬度增大、孔结构改善;蒸压养护还可能显著激发硅灰、石英粉和铁尾矿粉的火山灰活性,参与二次水化,生成结构...