以淀粉为碳源,正硅酸乙酯(TEOS)为硅源,通过溶胶-凝胶法制备了碳化硅前驱体淀粉-SiO2凝胶,将干凝胶在氩气氛中进行碳热还原制备碳化硅(SiC)。用XRD、IR、SEM、TEM及N2低温物理吸附等手段对合成的样品进行表征。结果表明,在淀粉-SiO2凝胶中添加镍催化剂在1450℃下就能合成出尺寸大小为40~60nm多孔高比表面积的纳米SiC,其孔径主要集中在4.2和10.6nm,比表面积为127.5m2/g,孔体积为0.43cm3/g。
Keyword:
Reprint 's Address:
Email:
Source :
功能材料
Year: 2009
Issue: 11
Volume: 40
Page: 1847-1849