Abstract:
采用十六烷基三甲基溴化铵(CTAB)作为模板剂,正硅酸乙酯(TEOS)为硅源,在碱性条件下,用低温合成方法合成了有序介孔硅,并以此为硬模板,蔗糖为碳前驱体,采用液相浸渍方法填充碳源,制备出有序介孔碳.通过XRD、TEM、N2吸附-脱附等测试方法对其表征,结果表明合成的介孔材料高度有序,均具有很高的比表面积(介孔硅,992~1096 m2/g;介孔碳,930~1208 m2/g),较大的孔容和较窄的孔径分布.还发现随着反应温度的升高,介孔硅的结构从二维六方相(p6mm)转变为三维立方相(Ia3d);介孔碳在复制介孔硅后,其结构也从三维立方相(Ia3d)转变为四方相(I41/a),并对相转变机理做了初步探讨.